ASTM G17-07-2020 طريقة الاختبار القياسية لمقاومة اختراق طلاءات الأنابيب (قضبان بلانت)

المعنى والاستخدام
3.1 As the pipe coating is subject to concentrated pressure exerted by the weight of the pipe and the backfill, the test is primarily used to determine the resistance of the coating to penetration or deformation under controlled conditions.

3.1.1 If the coating is not penetrated, the deformation of the compressible coating does not indicate a potential defect in the burial service. Deformation is not comparable to penetration of coating.

ASTM G17-07-2020 طريقة الاختبار القياسية لمقاومة اختراق طلاءات الأنابيب (قضبان بلانت)

يتراوح
1.1 This accelerated test method is used to determine the relative resistance of steel pipe coatings to penetration or deformation of blunt rods under specified loads. This test method is suitable for the test of all kinds of nonmetallic pipe coatings under various temperatures.

1.2 The value expressed in SI units with three significant decimals shall prevail. القيم الواردة بين قوسين هي للإشارة فقط.

1.3 وليس المقصود من هذا المعيار معالجة الجميع, لو اي, المخاوف المتعلقة بالسلامة المرتبطة باستخدامه. تقع على عاتق مستخدمي هذه المواصفة القياسية مسؤولية تحديد السلامة المناسبة, الممارسات الصحية والبيئية وتحديد إمكانية تطبيق القيود التنظيمية قبل الاستخدام.

1.4 This international standard is based on internationally recognized standardization principles established in the Decision on International Standards, Guidelines and Recommended Principles issued by the WTO Technical Barriers to Trade (TBT) لجنة.

شارك هذا المنشور