ASTM D7306-17 Pratique standard pour tester la formation de film à basse température des peintures au latex par observation visuelle

Signification et utilisation

5.1 Paint formulation designers can use this practice to determine whether a given paint has the ability to form a film at low temperatures. This practice can be used to help determine the level of coalescence solvent needed to form a good film. Test method D3793 compares the porosity of a film stretched at room temperature with another film stretched and cured at low temperatures.

5.2 This practice does not provide absolute information, but merely a ranking of the selected series of paints.

5.3 This practice can provide a pass-fail scenario if known acceptable and unacceptable coatings are included in the test.

ASTM D7306-17 Pratique standard pour tester la formation de film à basse température des peintures au latex par observation visuelle

Étape 1: Portée

1.1 This practice specifies a laboratory procedure for evaluating the ability of latex paints to form uniform films at low temperatures without apparent defects.

1.2 Les valeurs exprimées en unités SI doivent être considérées comme standard. Les valeurs données entre parenthèses sont à titre indicatif uniquement.

1.3 Cette norme n'est pas destinée à répondre à tous les problèmes de sécurité, si seulement, associé à son utilisation. Il est de la responsabilité des utilisateurs de cette norme d'établir des pratiques de sécurité et de santé appropriées et de déterminer l'applicabilité des restrictions réglementaires avant utilisation..

1.4 Cette norme internationale est basée sur les principes de normalisation internationalement reconnus établis dans le “Décision sur les principes pour l'élaboration de normes internationales, Lignes directrices et recommandations” publié par le Comité des obstacles techniques au commerce (OTC) de l'Organisation Mondiale du Commerce.

Partager cette publication