ASTM D5007-99-2017 “Metode Uji Standar Perubahan Daya Penutup Basah-Kering”

Arti dan kegunaannya
5.1 Banyak cat arsitektur, terutama cat putih dan terang, change significantly in film opacity as they dry. Increased coverage is sometimes associated with porosity and poor film integrity in conventional formulations. The reduction can lead to disappointing paint jobs. Karena itu, the change in covering power from wet to dry is a property of great practical significance.

5.2 This test method can be used for paint specifications and as a brief procedure for assessment and quality control.

ASTM D5007-99-2017 “Metode Uji Standar Perubahan Daya Penutup Basah-Kering”

jangkauan
1.1 This test method includes a visual assessment of wet and dry film to determine changes in the covering power of architectural coatings during drying.

1.2 This test method is not recommended for colors other than white and light colors.

1.3 The value in SI units shall prevail. Nilai yang diberikan dalam tanda kurung hanya untuk referensi.

1.4 Standar ini tidak dimaksudkan untuk mengatasi semuanya, jika ada, masalah keamanan yang terkait dengan penggunaannya. Pengguna standar ini bertanggung jawab untuk menetapkan praktik keselamatan dan kesehatan yang sesuai dan menentukan penerapan pembatasan peraturan sebelum digunakan..

1.5 Standar internasional ini didasarkan pada prinsip-prinsip standardisasi yang diakui secara internasional yang ditetapkan dalam Keputusan Prinsip-Prinsip Pengembangan Standar Internasional, Pedoman dan Rekomendasi yang dikeluarkan oleh Komite WTO tentang Hambatan Teknis Perdagangan (TBT).