- Beschrijving
- Navraag
Beschrijving
LR-100A Differential thermal analyzer
Product Introductie
DSC measures the relationship between temperature and heat flow related to the internal thermal transformation of materials, which has a very wide range of applications, especially material research and development, performance testing and quality control.Properties of materials such as glass transition temperature.Cold crystallization, phase transition, smeltend, crystallization, thermal stability, oxidation induction period, oxidation induction temperature, specific heat capacity, curing/crosslinking, are the research and development areas of DSC.
LR-100A Differential thermal analyzer
Belangrijkste kenmerken:
- New furnace body structure, good resolution and resolution and better baseline stability instrument master chip
- Digital gas flowmeter, control purge gas flow, data directly recorded in the database
- The instrument can adopt bidirectional control (host control, software control), friendly interface, makkelijk te besturen
- Using Cortex-M3 kernel ARM controller, faster processing speed, more temperature control
- USB two-way communication, convenient operation
- 7 inch 24bit full-color LCD touch screen, friendly interface
- Adopt professional alloy sensor
LR-100A Differential thermal analyzer
technische parameters:
1.DSC range: 0 ~ ±600mW
2.Temperatuurbereik: room temperature ~600℃
3.Verwarmingssnelheid: 0.1~100℃/min
4 temperature resolution: 0.01℃
5 temperature fluctuation: ±0.01℃
6.Temperature repeatability: ±0.1℃
7 DSC noise: 0.01μW
8.DSC resolution: 0.01μW
9.DSC: 0.01 mW
10.DSC sensitivity: 0.001mW
11.Temperatuurregelmodus: automatic control of the whole program
12.Curve scanning: heating scanning
13.Atmosphere control: automatic instrument switching
14.Weergavemodus: 24bit color, 7 inch LCD touch screen display
15.Data interface: standard USB interface
16.Parameter standard: equipped with standard material, with a key calibration function, users can correct the temperature and entha