LR-300 Differential Scanning Calorimeter
- Descrição
- Investigação
Descrição
LR-300 Differential Scanning Calorimeter
Introdução do produto:
LR-300 is the company launched DSC series of products with the highest accuracy of one, the sensor is the use of imported material E-couple, alta precisão, alta sensibilidade, good repeatability, signal acquisition circuit shielding protection, strong anti-interference, baseline stability and repeatability is very high.
LR-300 differential scanning calorimeter, can be glass transition temperature, phase transition temperature, melting point, enthalpy value, curing temperature and product stability, oxidation induction period and other tests. It is qualified for the research of pipe, polymer, químico, comida, medical and other fields, and serves universities, empreendimentos, third-party measurement and quality inspection units, with a wide range of applications to meet the testing needs of various industries.
LR-300 Differential Scanning Calorimeter
Parâmetros técnicos:
1.Faixa de temperatura: room temperature ~550℃
2 temperature resolution: 0.001℃
3 temperature fluctuation :±0.001℃
4.Temperature repeatability :±0.01℃
5.Taxa de aquecimento: 0.1 ~ 80℃/min
6.Constant temperature time: program setting ≤24h
7.Temperature control mode: aquecimento, Temperatura constante, resfriamento (automatic program control)
8.DSC range: 0 ~ ±600mW
9.DSC resolution: 0.01uW
10.DSC sensitivity: 0.001mW
11.Fonte de energia: AC220V/50Hz or customized
12.Atmosphere control gas: nitrogen, oxigênio (program setting/automatic switch)
13.Gas flow: 0-300ml /min
14 gas pressure: 0.2mpa
15.Modo de exibição: 24bit color, 7 inch LCD touch screen display
16.Interface de dados: standard USB interface
17.Parameter standard: equipped with standard material (indium, tin), users can adjust the temperature by themselves
18.The instrument has multiple groups of thermocouples, one group to measure sample temperature, one group to measure furnace body temperature, and one group to measure internal environment temperature
19.Cooling device: air cooling device (optional semiconductor & LT; – 40 ~ 550 ℃ & gt; Liquid nitrogen refrigeration < – 150 ~ 550 ℃ & gt;)
LR-300 Differential Scanning Calorimeter
Technical features:
- Industrial grade 7 tela sensível ao toque de polegadas, display rich information
- New furnace body structure, better baseline, higher accuracy. Heating adopts indirect conduction mode, high uniformity and stability, reduce pulse radiation, better than the traditional heating mode.
3.USB communication interface, strong commonality, reliable communication without interruption, support self-recovery connection function.
- Automatic switching of two air flow, fast switching speed, short stability time. Ao mesmo tempo, a protective gas input is added.
- Software is simple and easy to operate.
- Ultra-high sensitivity, precisão, 0.001 MW, 0.001℃
- Exquisite technical indicators, superior performance, cost-effective, widely used