ASTM G17-07-2020 Стандартный метод испытаний покрытий труб на стойкость к проникновению (Тупые стержни)

Значение и использование
3.1 As the pipe coating is subject to concentrated pressure exerted by the weight of the pipe and the backfill, the test is primarily used to determine the resistance of the coating to penetration or deformation under controlled conditions.

3.1.1 If the coating is not penetrated, the deformation of the compressible coating does not indicate a potential defect in the burial service. Deformation is not comparable to penetration of coating.

ASTM G17-07-2020 Стандартный метод испытаний покрытий труб на стойкость к проникновению (Тупые стержни)

диапазон
1.1 This accelerated test method is used to determine the relative resistance of steel pipe coatings to penetration or deformation of blunt rods under specified loads. This test method is suitable for the test of all kinds of nonmetallic pipe coatings under various temperatures.

1.2 The value expressed in SI units with three significant decimals shall prevail. Значения, указанные в скобках, предназначены только для справки..

1.3 Настоящий стандарт не предназначен для рассмотрения всех, если таковые имеются, проблемы безопасности, связанные с его использованием. Пользователи настоящего стандарта несут ответственность за установление соответствующей безопасности., практики в области здравоохранения и окружающей среды, а также для определения применимости нормативных ограничений перед использованием..

1.4 Этот международный стандарт основан на международно признанных принципах стандартизации, установленных в Решении о международных стандартах., Guidelines and Recommended Principles issued by the WTO Technical Barriers to Trade (ТБТ) комитет.

Поделиться этой записью