ASTM D7306-17 Standard Practice for Testing Low Temperature Film Formation of Latex Paints by Visual Observation

ความหมายและการใช้งาน

5.1 Paint formulation designers can use this practice to determine whether a given paint has the ability to form a film at low temperatures. This practice can be used to help determine the level of coalescence solvent needed to form a good film. Test method D3793 compares the porosity of a film stretched at room temperature with another film stretched and cured at low temperatures.

5.2 This practice does not provide absolute information, but merely a ranking of the selected series of paints.

5.3 This practice can provide a pass-fail scenario if known acceptable and unacceptable coatings are included in the test.

ASTM D7306-17 Standard Practice for Testing Low Temperature Film Formation of Latex Paints by Visual Observation

ขั้นตอน 1: ขอบเขต

1.1 This practice specifies a laboratory procedure for evaluating the ability of latex paints to form uniform films at low temperatures without apparent defects.

1.2 ค่าที่แสดงเป็นหน่วย SI ถือเป็นค่ามาตรฐาน. ค่าที่ระบุในวงเล็บมีไว้เพื่อการอ้างอิงเท่านั้น.

1.3 มาตรฐานนี้ไม่ได้มีวัตถุประสงค์เพื่อจัดการกับข้อกังวลด้านความปลอดภัยทั้งหมด, ถ้ามี, ที่เกี่ยวข้องกับการใช้งาน. เป็นความรับผิดชอบของผู้ใช้มาตรฐานนี้ในการกำหนดแนวทางปฏิบัติด้านความปลอดภัยและสุขภาพที่เหมาะสม และเพื่อพิจารณาการบังคับใช้ข้อจำกัดด้านกฎระเบียบก่อนใช้งาน.

1.4 มาตรฐานสากลนี้ตั้งอยู่บนหลักการมาตรฐานที่ได้รับการยอมรับในระดับสากลซึ่งกำหนดขึ้นใน “การตัดสินใจเกี่ยวกับหลักการพัฒนามาตรฐานสากล, แนวปฏิบัติและข้อเสนอแนะ” ออกโดยคณะกรรมการว่าด้วยอุปสรรคทางเทคนิคต่อการค้า (จะแจ้งภายหลัง) ขององค์การการค้าโลก.