ASTM D 3793-2006 ラテックス塗膜の低温重合

意味と目的
The test method does not provide absolute information, ただし、ランク付けされるのは選択したペイント シリーズのみです.

This test method can provide a pass-fail situation if the test contains known acceptable and unacceptable paint.

ASTM D 3793-2006 ラテックス塗膜の低温重合

の範囲
1.1 This test method consists of determining the comparative coalescence of a series of latex paints by measuring the porosity of films dried at standard and low temperatures. Porosity was assessed using a penetrating medium as shown in test method D 3258.

1.2 The texture of the film will affect the cleaning and the test results. A stain applied to a high shading paint does not reduce the reflectivity as much as the same stain applied to a low shading paint with equal porosity. These points need to be considered when comparing different paints.

1.3 This method should only be applied to comparative tests within one laboratory, as numerical results obtained in different laboratories are usually inconsistent.

1.4 SI単位で表した値を基準とします。. 括弧内の値は参考値です。.

この規格は、すべての安全上の懸念に対処することを目的としたものではありません, もしあれば, その使用に関連する. 適切な安全衛生慣行を確立し、使用前に規制上の制限の適用可能性を判断することは、この規格のユーザーの責任です。.