ASTM D 3793-2006 Polymerisatie bij lage temperatuur van latexverffilms

Betekenis en doel
The test method does not provide absolute information, maar rangschikt alleen de geselecteerde verfseries.

This test method can provide a pass-fail situation if the test contains known acceptable and unacceptable paint.

ASTM D 3793-2006 Polymerisatie bij lage temperatuur van latexverffilms

Reikwijdte van
1.1 This test method consists of determining the comparative coalescence of a series of latex paints by measuring the porosity of films dried at standard and low temperatures. Porosity was assessed using a penetrating medium as shown in test method D 3258.

1.2 The texture of the film will affect the cleaning and the test results. A stain applied to a high shading paint does not reduce the reflectivity as much as the same stain applied to a low shading paint with equal porosity. These points need to be considered when comparing different paints.

1.3 This method should only be applied to comparative tests within one laboratory, as numerical results obtained in different laboratories are usually inconsistent.

1.4 Waarden uitgedrukt in SI-eenheden worden als normen beschouwd. De waarden tussen haakjes zijn alleen ter referentie.

Deze norm is niet bedoeld om alle veiligheidsproblemen aan te pakken, indien aanwezig, die verband houden met het gebruik ervan. Het is de verantwoordelijkheid van gebruikers van deze norm om passende veiligheids- en gezondheidspraktijken vast te stellen en voorafgaand aan gebruik de toepasbaarheid van wettelijke beperkingen te bepalen..