ASTM D7306-17 Standard Practice for Testing Low Temperature Film Formation of Latex Paints by Visual Observation

Значење и употреба

5.1 Paint formulation designers can use this practice to determine whether a given paint has the ability to form a film at low temperatures. This practice can be used to help determine the level of coalescence solvent needed to form a good film. Test method D3793 compares the porosity of a film stretched at room temperature with another film stretched and cured at low temperatures.

5.2 This practice does not provide absolute information, but merely a ranking of the selected series of paints.

5.3 This practice can provide a pass-fail scenario if known acceptable and unacceptable coatings are included in the test.

ASTM D7306-17 Standard Practice for Testing Low Temperature Film Formation of Latex Paints by Visual Observation

Корак 1: Обим

1.1 This practice specifies a laboratory procedure for evaluating the ability of latex paints to form uniform films at low temperatures without apparent defects.

1.2 Вредности изражене у СИ јединицама сматрају се стандардним. Вредности дате у заградама су само за референцу.

1.3 Овај стандард није намењен да реши све безбедносне проблеме, ако их има, повезана са његовом употребом. Одговорност корисника овог стандарда је да успоставе одговарајуће безбедносне и здравствене праксе и да утврде применљивост регулаторних ограничења пре употребе.

1.4 Овај међународни стандард је заснован на међународно признатим принципима стандардизације утврђеним у “Одлука о принципима за развој међународних стандарда, Смернице и препоруке” издао Комитет за техничке баријере у трговини (ТБТ) Светске трговинске организације.