意义和目的
4.1 湿膜厚度测量有助于预测干膜厚度. Wet film thickness is usually specified in cases where dry film thickness cannot be measured nondestructively. 此外, the ability to determine the wet film thickness during the application can provide the opportunity to correct the application.

范围
1.1 This test method includes the determination of wet film thickness of organic coatings such as paint, varnisher and lacquer. The two methods are described as follows:

1.1.1 In test method A, wet film thickness was measured using a wet film thickness gauge (in imperial or metric scale (看 5.1)) up to 60 mils in the imperial scale series and 700 μm in the metric scale series (Sections 5 — 8).

1.1.2 In test Method B, the Pfund Gage was used to measure wet film thickness up to 14.2 密耳 (360 micmeters) (Sections 9-13).

ASTM D1212-2020 有机涂层湿膜厚度测量的标准测试方法

1.2 以 SI 单位表示的值被视为标准值. 括号内的数值仅供参考.

1.3 本标准并非旨在解决所有安全问题, 如果有的话, 与其使用相关. 本标准的使用者有责任建立适当的安全机制, 健康和环境实践,并在使用前确定监管限制的适用性.

1.4 本国际标准是根据技术性贸易壁垒委员会的决定中确立的国际公认的标准化原则制定的 (技术性贸易壁垒) 世界贸易组织关于制定国际标准的意见, 指导方针和推荐原则.