ASTM D5007-99-2017 “Standaard testmethode voor veranderingen in nat-droog dekvermogen”

Betekenis en gebruik
5.1 Veel architectonische verven, vooral witte en lichte verven, change significantly in film opacity as they dry. Increased coverage is sometimes associated with porosity and poor film integrity in conventional formulations. The reduction can lead to disappointing paint jobs. Daarom, the change in covering power from wet to dry is a property of great practical significance.

5.2 This test method can be used for paint specifications and as a brief procedure for assessment and quality control.

ASTM D5007-99-2017 “Standaard testmethode voor veranderingen in nat-droog dekvermogen”

bereik
1.1 This test method includes a visual assessment of wet and dry film to determine changes in the covering power of architectural coatings during drying.

1.2 This test method is not recommended for colors other than white and light colors.

1.3 The value in SI units shall prevail. De waarden tussen haakjes zijn alleen ter referentie.

1.4 Deze standaard is niet bedoeld om iedereen te behandelen, indien aanwezig, veiligheidsproblemen die verband houden met het gebruik ervan. Het is de verantwoordelijkheid van gebruikers van deze norm om passende veiligheids- en gezondheidspraktijken vast te stellen en voorafgaand aan gebruik de toepasbaarheid van wettelijke beperkingen te bepalen..

1.5 Deze internationale norm is gebaseerd op de internationaal erkende standaardisatieprincipes die zijn vastgelegd in het Besluit over de beginselen voor de ontwikkeling van internationale normen, Richtlijnen en aanbevelingen uitgegeven door het WTO-comité voor technische handelsbelemmeringen (TBT).